ISO 6383-1 Tear Resistance Plastic Film and Sheeting
This method is used to investigate the tear resistance of plastic films or sheets, less than 1 mm thick, in the form of a standard trouser-shaped test specimen.
The ISO 6383-1 test method is suitable for use with:
Film and sheeting of both flexible and rigid materials, provided that the material is not so rigid that a brittle fracture occurs during the test.
In principle, the test specimen is carefully clamped and aligned with the specimen legs in the grips so that the major axis coincides with an imaginary line joining the center of the grips. This is pulled apart until failure at a constant rate of displacement. The load is recorded as the tear propagates through the entire unslitlength of the specimen. The average force required to tear the specimen completely along its length is used to calculate the tear resistance of the material.
We use screw action grips, pneumatic action grips with rubber coated jaw faces for clamping of the material fitted to a tensile testing machine, normally a single-column or dual-column table-top design. Using a materials testing software, such as Bluehill®, allows you to input specimen details, set the desired test control, automatically calculate the desired results and statistics, and produce a test report all in accordance with the standard.
We suggest reviewing ISO 6383-1 to fully understand the test fixture and results requirements
3400 Series Universal Testing Systems Brochure
Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.
- Prodotti
- 06/27/2022
- 2.69 MB
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Prodotti
- 02/10/2020
- 4.15 MB
Bluehill Universal Brochure
Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.
- Prodotti
- 02/26/2017
- 3.76 MB
2710 Series Screw Side Action Grips
Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.
- Prodotti
- 06/28/2017
- 1.29 MB