ISO » ISO 9073-4 Tear Resistance Nonwovens

ISO 9073-4 Tear Resistance Nonwovens

This standard specifies a procedure to determine the tear force of nonwoven textile fabrics using the trapezoid method. A rectangular specimen is marked and prepared so that it can be loaded in the grip faces at an angle, allowing a tear to propagate across the specimen.

For this test, it is important to have an increased test data rate to ensure the capture a high number of data points. This is because when individual fibers within the fabric fail, the data rate must be fast enough to catch these peaks.

Pneumatic side action grips with rubber coated jaw faces are well suited for clamping of the trapezoid specimens. While manual action grips will work, many prefer pneumatic side action grips for ease of use, productivity, and better repeatability. Adjustable grip pressure also allows users to fine-tune the gripping pressure to avoid jaw breaks or slippage.

The challenges of testing to this standard are:

  • Rapid data capture rate
  • Specimen gripping




Instron's Solution:

  • Rapid data capture rate with Instron's 5900 controller allows data peaks and valleys to be captured accurately at up to 2,500 points per second
  • Instron pneumatic side action grips with rubber faces are well-suited to gripping nearly all types of fabric specimens for this test while maintaining high throughput

It is important to review ISO 9073-4:1997 in order to fully understand the test setup, procedure, and results requirements.

Literature

2712-04x Series Pneumatic Side Action Grips Data Sheet

Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.

  • Produits
  • 03/22/2022
  • 1.13 MB

2710 Series Screw Side Action Grips

Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.

  • Produits
  • 06/28/2017
  • 1.29 MB

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • Produits
  • 02/10/2020
  • 4.15 MB

3400 Series Universal Testing Systems Brochure

Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.

  • Produits
  • 06/27/2022
  • 2.69 MB

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Produits
  • 02/26/2017
  • 3.76 MB