Instron testing systems are designed to meet the these challenges– Like Suitable Strain Measurement, Impact Testing High-Strength Materials, Testing Full Section Pipe/Tube, Specimen Geometry– as the Pipe and Tube Industry moves towards the facilitation of global standarization.
Anwendungen 05/01/2014 1.84 MB

Effect of Frame Alignment on Tensile Strength of Unidirectional Carbon Fiber Laminates
Alignment has always been known to influence results from mechanical testing, but the effect on composites testing can be very significant. Many ASTM and ISO standards include recommendations regarding alignment, and auditing organizations mandate that the alignment is within defined limits. Ensuring good test alignment requires high-quality testing frames, grips, and fixtures, as well as the expertise to validate the alignment. Some companies choose not to align their test frame because they feel that the cost is too high and they believe that the effect on their results is minimal. Read our study that demonstrates the huge impact that alignment can have on test results and the effect that this can have on your company’s bottom line.
Whitepapers 04/30/2014 515.18 KB

A Review of Current In-Plane Composites Compression Testing
The compressive modulus and/or strength of a composite material are critical parameters for many structural uses. The factors that determine the compression strength are complex and the values of compressive strength for a composite can be much lower than values for tensile strength. One of the challenges in the compression testing of composite laminates is in understanding the various test types and standards. This white paper seeks to document and explain this field.
Whitepapers 04/30/2014 580.64 KB

Composites Test Fixtures: Open Hole Compression
Composite Test Fixtures Open-Hole Compression testing is preformed on multi-directional polymer matrix composite laminates reinforced with high modulus fibers.
Produkte 03/26/2014 174.68 KB

LigaGen: A Tension Bioreactor System
As documented in „Tissue Engineering Part A“, the Instron LigaGen Bioreactor was used in developing a tissue-engineered alternative to human hand tendons.
Press Releases 03/19/2014 49.28 KB

Instron Verification and Calibration Services in North America
We offer an extensive range of verification services in addition to force including strain, speed, displacement, alignment, impact, torque, temperature, and hardness, as well as dimensional verification of impact and CEAST® system components. Many of our calibration and verification services are available for non-Instron materials testing equipment.
Services 03/13/2014 2.78 MB

NEUE VERSION DER INSTRON® MPX PENDELSCHLAGWERKE FÜR DIE SICHERE UND EFFIZIENTE PRÜFUNG VON METALLEN NACH CHARPY UND IZOD
Die motorbetriebenen Pendelschlagwerke der Serie MPX von Instron, einem führenden Hersteller von Prüfsystemen zur Bestimmung der mechanischen Eigenschaften von Werkstoffen und Bauteilen, sind
speziell auf die Pendelschlagprüfung von Metallen nach Charpy und Izod ausgelegt. Die verfügbaren Schlagenergien reichen von 300 bis 900 Joules. Teil des Prüfsystems ist die Fracta™ Software zur
einfachen Datenerfassung und Berechnung der Schlagenergie. Bei höheren Ansprüchen an die Analyse und Protokollierung der Messdaten erlaubt ein Upgrade auf eine instrumentierte Charpy-Schlagfinne
und die Impulse™ Datenerfassungssoftware eine direkte Messung von Schlagkraft und Hammergeschwindigkeit.
Press Releases 03/12/2014 32.18 KB

Lap Shear Fixtures
The Lap Shear fixture, for use with Precision Manual Wedge Grips, provides a simple way of ensuring consistent alignment and hence repeatable lap shear test results.
Produkte 03/03/2014 646.44 KB

Kraftaufnehmer oder Druckaufnehmer
Bei diesem „White Paper“ handelt es sich um eine vergleichende Analyse, in der die Vorzüge von Kraftaufnehmern gegenüber Druckaufnehmer erläutert werden.
Produkte 02/26/2014 187.5 KB

VisualRHEO | Software for CEAST SR Series Capillary Rheometers
A fundamental part of a capillary rheometer system is the software. As the system investigates the flow behavior of
plastics over a wide range of shear conditions, the software controls the instrument from a PC, acquiring and analyzing
data, calculating results, and exporting data to easily share and perform further analysis. Performing tests that are much
more effective and informative than a trial-and-error approach, the software provides a user-friendly interface for lab
operators when programming and monitoring the tests.
Produkte 02/14/2014 2.46 MB