Products » Testing Accessories » Axial Clip-on » 2620 Series Dynamic Strain Gauge Extensometers » Dynamic Extensometer 12.5mm GL ±5mm Travel

Dynamic Extensometer 12.5mm GL ±5mm Travel

Catalog no. 2620-601

2620-601 | Dynamic Extensometer 12.5mm GL ±5mm Travel

Dynamic Extensometer for direct strain measurement and closed loop strain control. Suitable for tensile, compressive & fatigue testing, the extensometer has a 12.5mm gauge length with a travel of ±5mm giving ±40% strain.

It includes a 12.5mm extender to give a gauge length of 25mm and ±20% strain and a 37.5mm extender to give a gauge length of 50mm and strain of ±10%.

Temperature range: -80C to +200C. Compatible with 8800 and 8500Plus controllers. May be immersed in acetone, silicone or alcohol.

Specifications
Accessory Height 63 mm (2,48 in)
Accessory Weight 0,02 kg (0,044 lb)
Accessory Width 21 mm (0,83 in)
Gauge Length 12,5 ; 25 et 50 mm (0.49, 0.98 et 1.97 in)
Specimen Diameter 3 - 25 mm (0.12 à 1 in)
Specimen Thickness 3 - 12,5 mm (0,12 - 0,5 in)
Specimen Width 0 - 25 mm (0 - 1 in)
Static or Fatigue Rated Fatigue
Temperature Rating -80 à +200 °C (-112 à +392 °F)
% Travel (Axial) ±40, ±20 et ±10 %

 

Literature