Products » Testing Accessories » Axial Clip-on » 2620 Series Dynamic Strain Gauge Extensometers » Dynamic Extensometer 25mm GL +12.5mm -2.5mm Travel

Dynamic Extensometer 25mm GL +12.5mm -2.5mm Travel

Catalog no. 2620-604

2620-Series_P
2620-Series_P

2620-604 | Dynamic Extensometer 25mm GL +12.5mm -2.5mm Travel

Dynamic Extensometer for direct strain measurement and closed loop strain control. Suitable for tensile, compressive & fatigue testing, the extensometer has a 25mm gauge length with a travel of +12.5mm to -2.5mm giving +50% to -10% strains.

It includes an extender to give a gauge length of 50mm and strain of +25% to -5% strain.

Temperature range: -80°C to +200°C. Compatible with 8800 and 8500Plus controllers.

May be immersed in acetone, silicone or alcohol.

Specifications
Accessory Height 69 mm (2.72 in)
Accessory Weight 0.02 kg (0.044 lb)
Accessory Width 21 mm (0.83 in)
Gauge Length 25 and 50 mm (0.98 and 1.97 in)
Specimen Diameter 3 – 25 mm (0.12 – 1 in)
Specimen Thickness 3 – 12.5 mm (0.12 – 0.5 in)
Specimen Width 0 – 25 mm (0 – 1 in)
Static or Fatigue Rated Fatigue
Temperature Rating -80 to +200°C (-112 to +392°F)
% Travel (Axial) +50 to -10% and +25 to -5%