Applications of HDT and Vicat Tests
If you are into Automotive and Injection molding, you might need to evaluate the HDT/Vicat thermo-mechanical properties of your material and test it according to ASTM D648 and ISO 75, ASTM D1525 and ISO 306.
Today we want to take a look at HDT/MV cut tests. I'm Saverio, Application Engineer at Instron, here to tell you all about it.
HDT and Vicat tests are very well-known tests to measure the performance of a plastic in high‑temperature applications. The top three application scenarios for HDT and Vicat tests are injection‑molded plastic parts for metal replacement. That has been one of the top trend topics in the last decade for automotive applications. In the future we will also certainly see more applications for EV batteries, so all related polymers in the process need to be characterized.
Finally, automotive interior design is influenced by proportion, shape, placement, and surfaces, so the smoothness, the feel, but also the stiffness are just a few parameters to be considered during the material characterization when developing such parts.
Here we have a polypropylene‑based specimen that I'm going to test. This material is typically used for car dashboards. On a hot summer day, temperature of the dashboard can easily reach 50 degrees C, so if the material used to make such dashboards has not been tested at these conditions, then the dashboard can easily deform and suffer damages. HDT and Vicat values mean that the sample has been tested under these conditions and thus is useful for high‑temperature applications.
For my test I'm going to use an Instron HV3S machine that is equipped with three stations. This machine can contain up to 12 liters of silicone oil, and for my test I filled it with medium‑temperature silicone oil as I expect to reach up to 140 degrees C. Innovative features such as the maximum oil temperature control, the oil level control, and the oil degradation control monitor the oil throughout the test, reducing the risk of running invalid tests.
The Touch display guides me through the entire testing process with step‑by‑step instructions. These ensure that the tests are error‑free, simple, and repeatable. The predefined ISO and ASTM templates enable me to run tests in a few simple touches. With BlueHV software I can be guided as well, but I can also recollect additional information such as the real displacement plot against real time.
What I'm going to do is simply go to the test section, select the already created method, follow the tab instructions one by one, load the weights onto the station, and then click to have the test started.
The test can last hours, and after the test is completed the results are displayed and ready to be analyzed.
That's all for today. If you'd like to know more about our testing solutions, please feel free to contact us.