ISO 18489 Cracked Round Bar Test Method

In long term applications of thermoplastic materials such as polyethylene (PE) pipes or fittings it is important to rank and pre-select materials based on their resistance to long-term failure mechanics as a result of slow crack growth (SCG). Developments in modern raw materials has led to a significant increase in resistance of PE to crack initiation and SCG so that testing with previous methods exceeded practical time frames. ISO 18489 achieves a significant reduction in testing time at ambient temperatures more relevant to the temperature range of many applications and that do not change the structural status of the polymer. Acceleration of material testing is achieved by specimen geometry and cyclic loading regime resulting in a relatively short test time.

CHALLENGE - TESTING TO ISO18489 CRACKED ROUND BAR TEST METHOD

  • Need to determine long-term failure mechanics as a result of crack initiation and slow crack growth
  • Cylindrical specimens notched and cyclically loaded to failure, avoid static loading pre-test, may cause creep at notch tip
  • Number of cycles to failure recorded as function of stress range

SOLUTION - ELECTROPULS E3000 - DETERMINATION OF RESISTANCE TO SLOW CRACK GROWTH UNDER CYCLIC LOADING

  • Capable of imposing and recording cyclic load varied by time between accurately defined limits, constant values +/- 1%
  • Determines resistance of PE material to slow growing brittle cracks
  • Quickly predict life expectancy of pipe
  • Custom fixture designed and developed with customer

THE INSTRON ADVANTAGE

  • Multiple operators produce repeatable and reliable results, made possible with the patented stiffness based tuning
  • ElectroPuls is a reliable test instrument that can be run uninterrupted with no need to stop and restart, saving time and hassle of preparing new samples
  • Confidence in data through accurate loading during test across a range of frequencies
Literature

ElectroPuls

With more than ten years of running tests over billions of cycles, ElectroPuls systems are the established materials testing machines using patented linear motor technology. With model capacities up to 20 kN, ElectroPuls systems offer slow-speed static testing and high-frequency dynamic fatigue testing with hundreds of hertz capability. The Linear-Torsion models feature a patented actuator for bi-axial tests on materials and components.

  • Products
  • 06/05/2019
  • 3.63 MB

ElectroPuls® E1000 All-Electric Dynamic Test Instrument

The ElectroPuls® E1000 is a state-of-the-art, all-electric test instrument designed for dynamicand static testing on a wide range of materials and components. It includes Instron® advanceddigital control electronics, DynacellTM load cell, Console software, and the very latest in testingtechnology – hassle-free tuning based on specimen stiffness, electrically operated crossheadlifts, a T-slot table for flexible test set ups, and a host of other user-orientated features. Poweredfrom a single-phase supply it requires no additional utilities for basic machine operation (forexample, pneumatic air, hydraulics, or water).