ISO Standards for Materials Testing » ISO 20795-1 and 20795-2 Flexure Test of Base Polymers

ISO 20795-1 and 20795-2 Flexure Test of Base Polymers

Dental restorative and prosthodontics materials experience stresses caused by mastication action once they are in the mouth. Each dental material may respond to the stresses differently and in some cases, deformation can occur.  For example, the porcelain portion of the dental crown can chip or break off while biting down on hard food. Therefore, evaluating the mechanical properties of dental materials can be useful to establish their functions and predict the long-term clinical performance.

ISO 20795 Dentistry – Base Polymers Part 1: Denture-Base Polymers and Part 2: Orthodontic-Base Polymers specify the requirements for denture and orthodontic base polymers and copolymers used in dental applications. Test methods that are used to determine compliance with these requirements are also specified in the standards. One of the tests is the three-point flexure test, which measures the ultimate flexure strength and modulus of the polymers using 3.2 mm diameter anvils placed 50 mm apart. For instance, in accordance to ISO 20795-1, dental cements of type 1, 3, 4, and 5 should have minimum ultimate flexure strength of 65 MPa for at least 4 out of 5 tested specimens.

To meet the requirements of ISO 20795-1, we used a custom 3-point flexure fixture with a temperature-controlled bath. The temperature of the specimen was maintained at 37° C (±1°) to simulate in-vivo conditions. The setup shown in the picture was mounted onto an ElectroPuls™ Test System and the test was controlled by our 3 Software®Bluehill. However, since this is a quasi-static test, it can also be easily carried out on either a 3300 or 5900 Electromechanical Testing Machine.

We recommend that you review ISO 20795 to fully understand its requirements.

Interested in other types of test for dental materials or dental implants? We have a variety of solutions for testing of dental materials and implants.

Literature

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • Products
  • 02/10/2020
  • 4.15 MB

ElectroPuls® E1000 All-Electric Dynamic Test Instrument

The ElectroPuls® E1000 is a state-of-the-art, all-electric test instrument designed for dynamicand static testing on a wide range of materials and components. It includes Instron® advanceddigital control electronics, DynacellTM load cell, Console software, and the very latest in testingtechnology – hassle-free tuning based on specimen stiffness, electrically operated crossheadlifts, a T-slot table for flexible test set ups, and a host of other user-orientated features. Poweredfrom a single-phase supply it requires no additional utilities for basic machine operation (forexample, pneumatic air, hydraulics, or water).

  • Products
  • 02/06/2025
  • 378.09 KB

ElectroPuls E3000®

The ElectroPuls® E3000 Linear-Torsion is a state-of-the-art, all-electric test instrument designed for dynamic and static testing on a wide range of materials and components. It includes Instron® advanced digital control electronics, bi-axial DynacellTM load cell, Console software, and the very latest in testing technology – hassle-free tuning based on specimen stiffness, electrically operated crosshead lifts, a T-slot table for flexible test set ups and a host of other user-orientated features. Powered from a single-phase supply it requires no additional utilities for basic machine operation (for example, pneumatic air, hydraulics, or water).

  • Products
  • 02/06/2025
  • 394.66 KB