Hoof pads are often used in conjunction with horseshoes to treat various pathologies within a horse's foot. Pad materials must be malleable enough to conform to the animal's foot while also strong enough to support its weight. This 1993 patent uses an Instron rheometer to analyze polymers for a new custom-fitting hoof pad.