ISO 844 Rigid Cellular Plastics Compression Properties
ISO 844 is used to investigate the compressive behavior of cellular plastics for determining the compressive strength, compressive strength at pre-defined deformations, compressive modulus, and other aspects of the compressive stress/strain relationship under the conditions defined.
In principle, the test specimen is centrally positioned between the two parallel anvils then compressed along its major axis at a constant rate of displacement until the specimen has deformed as a percentage of the specimen's original height. For this test type, we use the preload feature of Bluehill® Universal software to determine the anvil height. The load sustained by the specimen is measured during this procedure. To record the test it is important to have a high speed intelligent test data logging rate. This is the transfer rate to the PC of 100Hz or more to capture and record all data.
We used hardened-steel compression anvils used to apply the deformation load to the test specimen. These anvils are fitted to a tensile testing machine, usually of single-column or dual-column table-top design. Using testing software, such as our Bluehill Universal test method, is ideal for inputting specimen details, setting the desired test control, automatically calculating the desired results and statistics, and producing a test report all in accordance with the standard.
We suggest reviewing the official ISO 844 standard to fully understand the test fixture and results requirements.
3400 Series Universal Testing Systems Brochure
Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.
- Produits
- 06/27/2022
- 2.69 MB
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Produits
- 02/10/2020
- 4.15 MB
Bluehill Universal Brochure
Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.
- Produits
- 02/26/2017
- 3.76 MB
Plastics Testing Solutions Brochure
The Plastics Testing Solutions brochure is a 40-page, applications-focused, and standards-based brochure. Important standards such as ISO 527-1, -2, -3, ISO 11443, ISO 75, ASTM D638, ASTM D3835, are covered in a detailed testing challenge and solution format. The brochure addresses the most prominent and widely-used standards in the materials testing industry for plastics. Test types such as Impact, Rheology, Thermo-Mechanical, Specimen Preparation, Mechanical Testing, Dynamic/Fatigue, and Hardness are described in great detail.
- Applications
- 04/12/2024
- 12.48 MB