ISO Standards for Materials Testing » ISO 14130 Determination of Apparent Interlaminar Shear Strength by Short-Beam Method

ISO 14130 Determination of Apparent Interlaminar Shear Strength by Short-Beam Method

The ISO 14130 test method covers the determination of the apparent interlaminar shear strength (ILSS) of fiber-reinforced plastic composites by the short-beam method. The method is suitable for composites with either a thermoset or thermoplastic matrix. The data obtained is not suitable for determining the design parameters, but it can be used for screening materials or for quality control. So with the various test samples there will also be variation on the failure mode, which is dependent on the fiber lay-up procedures used during manufacturing.

Our CP110860 shear fixture consists of a bar of rectangular cross section with two supports which the sample is placed with the loading member midway between the supports. The fixure incorporates a guided upper anvil to ensure parallel loading of the specimen. This test procedure has a smaller test span and the specimen thickness ratio is adopted to increase the level of shear stress relative to the flexural stress in the test specimen to encourage interlaminar shear failure.

We recommend testing with either the 3400 or 6800 Universal Testing Instruments with our dedicated Bluehill® Universal software modules for this application, as it can easily be configured with any of the other common composite test applications, such as tensile, flexural, and compression.

We recommend reviewing the ISO 14130 in full to understand the test fixture and results requirements relevant to the materials you are testing.

Literature

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Products
  • 02/26/2017
  • 3.76 MB

Composite Test Fixtures | Flexural and Interlaminar Shear

Interlaminar shear testing is a simple test on easy to prepare polymer composite specimens that measures of the strength of the bond between fibers and matrix. Another common test for polymer composites is flexure testing. The Instron® Modular Flexural and Interlaminar Shear Strength (ILSS) bend fixture system, with a range of interchangeable anvils, is suitable for testing to a number of international standards, including ASTM D2344, D790, EN 2562, EN 2563, ISO 14125, and ISO 14130.

  • Products
  • 09/02/2014
  • 486.43 KB