Universal Testing Systems

Products » Testing Systems » Universal Testing Systems

Universal Testing Systems

Instron universal testing machines include electromechanical and hydraulic powered systems capable of performing static testing, including tensile, compression, bend, peel, tear, shear, friction, puncture, and other mechanical tests.

6800 Series Universal Testing Systems
6800 Series Universal Testing Systems

6800 Series Universal Testing Systems

Up to 300 kN Force Capacity

Designed for exceptional performance, the 6800 Series is Instron's most advanced universal testing system, delivering unparalleled accuracy, reliability, and superior alignment capable of meeting Nadcap requirements. All this is combined with improved ergonomics to offer an enhanced testing experience for today’s operator.

Instron 10 Year Mechanical Systems Warranty
OVERVIEW
Force Capacity Range 0.02 N (2 gf) to 300 kN
Load Measurement Accuracy ± 0.5% of Reading Down to 1/1000 of Load Cell Capacity  Load Measurement Accuracy:

± 0.5% of reading down to 1/1000 of load cell capacity with 2580 Series load cells

± 0.5% of reading to 1/250 of load cell capacity with 2525 or 2530 Series load cells

Data Acquisition Rate Up to 5000 Hz with Adjustable Bandwidth Control
Recommended For Advanced Testing, Complex Data Acquisition with Multiple Channels, High Throughput Demands, Highly Regulated Industries, Future Proofing
Features • Auto Positioning  Auto Positioning saves the correct fixture separation starting location for each test method. This ensures all operators run each test exactly the same way. Only available on 6800 Series systems.
• Specimen Protect  Specimen Protect prevents excessive forces from being applied to the specimen during setup, protecting your critical specimens from damage.
• Advanced Accessory and Automation Compatibility  The 6800 Series platform is compatible with all of Instron's advanced accessories, such as the AVE 2 non-contacting video extensometer and torsion add-on. The 6800 Series is also compatible with the latest automation solutions, including the CT6 cobot, AT2 automated XY stage, and AT3/AT6 automated testing systems.
• Automatic Gain Adjustment  Allows for closed loop strain control.
• Increased Axial Stiffness Compared to 3400 Series  The 6800 Series is built for high performance. It features pre-loaded bearings, precision ball screws, an extra thick crosshead and base beam, and low-stretch drive belts to ensure superior performance and longevity.
• Up To 13 Channels + Analog Output and Digital I/O Board  The 6800 Series can be expanded to include digital input/output channels and up to 11 sensor conditioning modules to ensure compatibility with advanced accessories and external devices.
• Removable Handset  The 6800 Series brings system controls closer than ever before with an all-new ergonomic handset, mounted directly to the frame. Operators can use the handset in the mounted position or removed from its dock.
• Collision Mitigation  Reduce damage to equipment and specimens by stopping the crosshead if a force is detected upon return or during a jog.
• Safety Coaching  Clear visual feedback regarding system status to notify operators when it is safe to enter the test space.
• Optional Smart-Close Air Kit  Finger pinch hazards from pneumatic grips are reduced through lower grip-closing pressure and restricted speed during the setup phase of your test.
• Frames with Height and Width Options  All 6800 Series frame styles (single column, table model, and floor models) are offered in extra height and width variants to accommodate oversized specimens and testing of high elongation materials.
Advanced Capabilities
Torsion Add-On The Torsion Add-On can be integrated with any new or existing 6800 Series system, allowing for simultaneous or independent axial and torsional testing.
Automated XY Stage The AT2 can be installed on any new or existing 6800 Series system to automate compression, tensile, and flexure testing of devices or components with multiple test points or multiple components with repetitive test points.
Multi-Station A multi-station system offers enhanced throughput with its ability to perform simultaneous, independent tests on up to five separate specimens using a single load frame.
Autoinjector Testing System Developed in close partnership with pharmaceutical companies and CDMOs, Instron’s Autoinjector Testing System provides full functionality testing in an all-in-one, easy to use package. Designed to address the requirements of ISO 11608, the Autoinjector Testing System makes it easy to run a complete sequence of tests on a single system.
3400 Series Universal Testing Systems
3400 Series Universal Testing Systems

3400 Series Universal Testing Systems

Up to 300 kN Force Capacity

The 3400 Series electromechanical universal testing machines offer the simplicity and performance needed for routine, standardized quality control tests and general-purpose mechanical testing.

Instron 10 Year Mechanical Systems Warranty
OVERVIEW
Force Capacity Range 0.025 N (2.5 gf) to 300 kN
Load Measurement Accuracy ± 0.5% of Reading Down to 1/250 of Load Cell Capacity  Load Measurement Accuracy:

±0.5% of reading down to 1/250 of load cell capacity

±1.0% of reading down to 1/500 of load cell capacity

Data Acquisition Rate Up to 1000 Hz
Recommended For Simple Testing
Features • Collision Mitigation  Reduce damage to equipment and specimens by stopping the crosshead if a force is detected upon return or during a jog.
• Safety Coaching  Clear visual feedback regarding system status to notify operators when it is safe to enter the test space.
• Optional Smart-Close Air Kit  Finger pinch hazards from pneumatic grips are reduced through lower grip-closing pressure and restricted speed during the setup phase of your test.
• Frames with Height Options  Select 3400 Series frame styles (single column and table models) are offered in extra height variants to accommodate testing of high elongation materials.

Automation for Universal Testing Systems

Instron offers a range of automation solutions for universal testing machines to improve throughput, repeatability, and safety, while freeing up skilled operators to focus on more complex and creative tasks. Available as either a complete turnkey solution or as modules that can be fitted to existing universal testing systems, Instron automation products can be tailored to your program’s specific requirements.

OVERVIEW
AT6 The AT6 system is built around a 6-axis robot capable of high-volume, round-the-clock testing, automating everything from specimen measurement to data collection and disposal, and can even integrate additional testing equipment such as Rockwell and Vickers hardness testers, durometers, and roughness testers.
AT3 With a relatively compact footprint, the AT3 is capable of holding up to 160 specimens and can automate the entire testing process from specimen measurement to data collection and disposal. The system is commonly configured for tensile, compression, flex, and lap shear testing to meet a range of international standards.
Automated XY Stage The AT2 can be installed on any new or existing 6800 or 5900 Series universal testing system to automate compression, tensile, and flexure testing of devices or components with multiple test points or multiple components with repetitive test points.
Automated Carousel The automated carousel testing system utilizes an innovative, adaptable design to automate batch testing – typically used for compressive type tests on medical vials, cartridges, and pre-filled syringes.
CT6 Cobot This system pairs a collaborative robot (cobot) with a 6800 or 5900 Series universal testing system to increase the efficiency of small to mid-sized testing labs that require a high degree of flexibility in their testing systems.
Multi-Station While not a traditional automation system, the 6800 Series multi-station system offers enhanced throughput with its ability to perform simultaneous, independent tests on up to five separate specimens using a single load frame.

5980 Series Universal Testing System
5980 Series Universal Testing System

5980 Series Universal Testing Systems

Up to 600 kN Force Capacity

The 5980 Series is a floor model platform that delivers the highest force capacity for Instron’s electromechanical universal testing systems. Offering up to 600 kN force for testing high-strength materials, the 5980 Series is capable of meeting stringent Nadcap alignment requirements.

OVERVIEW
Maximum Force Capacity Up to 600 kN
Load Measurement Accuracy ± 0.5% of Reading Down to 1/1000 of Load Cell Capacity  Load Measurement Accuracy:

± 0.4% of reading down to 1/100 of load cell capacity with 2525, 2530 or 2580 Series load cells

± 0.5% of reading down to 1/1000 of load cell capacity with 2580 Series load cells

± 0.5% of reading to 1/250 of load cell capacity with 2525 or 2530 Series load cells

Data Acquisition Rate Up to 2500 Hz with Adjustable Bandwidth Control
Recommended For Metal Alloys, Composites, and Other High Strength Materials
Features • Specimen Protect  Specimen Protect prevents excessive forces from being applied to the specimen during setup, protecting your critical specimens from damage.
• Advanced Accessory and Automation Compatibility  The 5980 Series platform is compatible with all of Instron's advanced accessories, such as the AVE 2 non-contacting video extensometer and torsion add-on. The 5980 Series is also compatible with the latest automation solutions, including the AT2 automated XY stage and AT3/AT6 automated testing systems.
• Automatic Gain Adjustment  Allows for closed loop strain control.
• Increased Axial Stiffness  The 5980 Series is built for high performance. It features pre-loaded bearings, precision ball screws, an extra thick crosshead and base beam, and low-stretch drive belts to ensure superior performance and longevity.
• Up To 13 Channels + Analog Output and Digital I/O Board  The 5980 Series can be expanded to include digital input/output channels and up to 11 sensor conditioning modules to ensure compatibility with advanced accessories and external devices.
• Removable Handset  The ergonomic handset brings system controls closer than ever before. Operators can use the handset in the frame mounted position or removed from its dock.

Industrial Series Universal Testing Systems

Up to 2000 kN Force Capacity

OVERVIEW
Maximum Force Capacity Up to 2000 kN
Load Measurement Accuracy ± 0.5% of Reading Down to 1/500 of Load Cell Capacity
Data Acquisition Rate Up to 1000 Hz
Recommended For Metal Alloys, Concrete, and Other High Strength Materials
Features • Specimen Protect  Specimen Protect prevents excessive forces from being applied to the specimen during setup, protecting your critical specimens from damage.
• Automatic Gain Adjustment  Allows for closed loop strain control.
• Removable Handset  The ergonomic handset brings system controls closer than ever before. Operators can use the handset in the frame mounted position or removed from its dock.
• Dual Test Space Design on Select Frames  The DX and HDX frames are designed for tension, compression, bend/flex, and shear testing without needing to remove application specific fixtures from the compression test space in order to perform tensile tests.
• Compatible with Advanced Extensometry  Including the AVE3 Advanced Video Extensometer, AutoX750 Automatic Contacting Extensometer, and all of Instron's other extensometer products.
Curved Needle Testing System with Bluehill Universal
Curved Needle Testing System with Bluehill Universal Curved Needle Testing 6800 Series System Custom Extra Tall 68FM Universal Testing System

Specialty Systems

Instron’s Engineered Solutions Group works closely with our customers to develop custom solutions to fit specific application requirements. The following does not represent a complete list of Instron’s specialty systems – please contact us to discuss your specific requirements.

OVERVIEW
Curved Needle Testing System The Curved Needle Testing System is designed for testing the needles used in wound closure and surgical procedures. It can be used to perform curved needle puncture testing per ASTM F3014 and cantilever bend testing. The curved needle puncture testing fixture is used to evaluate needle sharpness and coating durability, and the needle bend testing fixture is used to evaluate the flexural properties of a needle during use.
Common Customizations Instron universal testing systems can be customized to fit a wide range of application needs. This can include customized frame heights and widths to accommodate unique specimen dimensions and lab constraints; custom debris shields and light curtains for enhanced safety; custom high-speed frames to fit test requirements; and more.

Contact Our Sales Department.

Please complete the form below and we will be happy to contact you with a response. Our typical response time for an online request is within 1-2 business days. For a faster response, please call +1-800-473-7838.



Please close this window and accept cookies to view and fill out the form.
Instron 6800 series testing systems
Instron 6800 series testing systems SATEC systems are no longer in production Electromechanical testing systems that are no longer in production

Retrofits and System Upgrades

For Out of Production Universal Testing Systems

Many out of production Instron testing systems can be retrofitted with current componentry to maximize machine life and serviceability. Eligible systems can also be upgraded with the latest testing software for enhanced testing capabilities and efficiencies.

Types of Retrofits and Upgrades
Electromechanical Retrofits Eligible electromechanical testing systems can be modernized with the latest 3400 or 6800 Series control electronics and Bluehill Universal software. This upgrade enhances testing functionality and ensures compatibility with the latest testing accessories.
Static Hydraulic Retrofits Eligible static hydraulic testing systems can be retrofitted with 5900 Series control electronics and the latest Bluehill Universal software to enhance the system's functionality and enable compatibility with all the latest testing accessories.
Software Only Upgrade Depending on the electronics and PC operating system, certain testing systems are eligible for a software-only upgrade. This brings your software back to fully supported status and gives your lab access to all the latest software features and functionality available in Bluehill Universal.

To view the Product Life Cycle status of your system, and whether it’s eligible for a system retrofit or software upgrade, visit our out of production section — which lists previous generation systems dating back to our founding in 1946.